Reference | Alloy | Liquidus en °/C | Solidus en °/C | Density | |
4060 | In/99,99 | 156 | E | 156 | 7,31 |
4999 | In grenaille 99.9999 | ||||
4110 | In/Ag/970/30 | 143 | E | 143 | 7,38 |
4040 | In/Ag/950/50 | 162 | 159 | 7,42 | |
4000 | In/Ag/900/100 | 237 | 141 | 7,53 | |
4090 | In/Bi/950/50 | 72 | E | 72 | 7,99 |
4091 | In/Bi/663/337 | 150 | 125 | 7,40 | |
4092 | In/Bi/600/400 | 125 | 117 | 8,14 | |
4170 | In/Bi/Cd/620/300/80 | 62 | E | 62 | 8,02 |
4175 | In/Bi/Cd/617,2/307,8/75 | 61,5 | E | 61,5 | 8,03 |
4180 | In/Bi/Sn/510/330/160 | 61 | E | 61 | 7,98 |
4150 | In/Cd/740/260 | 123 | E | 123 | 7,62 |
4070 | In/Cu/990/10 | 153 | E | 153 | 7,32 |
4080 | In/Ga/993/7 | 150 | E | 150 | 7,30 |
4081 | In/Pb/810/190 | 160 | E | 160 | 7,84 |
4050 | In/Pb/750/250 | 170 | 162 | 8,02 | |
4035 | In/Pb/700/300 | 174 | 160 | 8,19 | |
4033 | In/Pb/600/400 | 185 | 174 | 8,52 | |
4010 | In/Pb/550/450 | 215 | E | 215 | 8,70 |
4030 | In/Pb/520/480 | 205 | 177 | 8,81 | |
4020 | In/Pb/500/500 | 209 | 180 | 8,89 | |
4100 | In/Pb/Ag/800/150/50 | 149 | E | 149 | 7,85 |
4160 | In/Sn/520/480 | 118 | E | 118 | 7,30 |
4161 | In/Sn/500/500 | 125 | 117 | 7,30 | |
4165 | In/Sn/Cd/440/420/140 | 93 | E | 93 | 7,46 |
4120 | In/Sn/Pb/400/400/200 | 130 | 121 | 7,86 | |
4140 | In/Sn/Pb/Cd/700/150/96/54 | 125 | E | 125 | 7,63 |